Basic Compounds for Superalloys

Basic Compounds for Superalloys

EnglishPaperback / softbackPrint on demand
Pelleg Joshua
Elsevier Science Publishing Co Inc
EAN: 9780128161333
Print on demand
Delivery on Thursday, 13. of August 2026
CZK 4,590
Common price CZK 5,100
Discount 10%
pc
Do you want this product today?
Megabooks Praha Korunní
not available
Librairie Francophone Praha Štěpánská
not available
Megabooks Ostrava
not available
Megabooks Olomouc
not available
Megabooks Plzeň
not available
Megabooks Brno
not available
Megabooks Hradec Králové
not available
Megabooks České Budějovice
not available
Megabooks Liberec
not available

Detailed information

Basic Compounds for Superalloys: Mechanical Properties explores the mechanical properties of the iron group based intermetallic compounds that are the basis of super-alloys. Chapters explore tensile tests and compressive stress and hardness and provide detailed considerations that are devoted to time dependent deformation, namely creep and cyclic deformation. In addition, a discussion of the nano-crystalline L12 and B2 structures and their mechanical properties is included. Fracture and failure of these materials in both macro and nano-iron based compounds is also considered. This book is ideal for engineers, scientists and technical personnel who work in materials engineering, materials science, and mechanical and chemical engineering.
EAN 9780128161333
ISBN 0128161337
Binding Paperback / softback
Publisher Elsevier Science Publishing Co Inc
Publication date June 22, 2018
Pages 624
Language English
Dimensions 229 x 152
Country United States
Readership Professional & Scholarly
Authors Pelleg Joshua
Manufacturer information
The manufacturer's contact information is currently not available online, we are working intensively on the axle. If you need information, write us on [email protected], we will be happy to provide it.